News Centre
News Type
Send your inquiry
Plastics for Lithium-Ion Battery Manufacturing Equipment
Process Stations and Their Material Demands
Station | Environment | Material |
Electrode coating & drying | NMP solvent, 120–150°C | PEEK, PPS, PTFE-lined components |
Calendering | High pressure, clean surface | PEEK, PI for rolls and guides |
Slitting & die cutting | Abrasion, burr control | POM, PEEK, PU rollers |
Stacking & winding | Precision, no contamination | PEEK, POM, PPS, ceramic-filled grades |
Electrolyte filling | Corrosive solvent, moisture-critical | PTFE, PFA, PVDF, PP |
Laser welding & sealing | Heat, precise location | PEEK, PPS, PI fixtures |
Formation & ageing racks | Electrical insulation, heat | PPS, PBT, PEEK insulators |
The Dry Room Constraint
Cell assembly happens at dew points below −40°C in many plants, and that environment strips moisture from everything — including polymers. Materials that rely on absorbed water for antistatic performance stop working entirely in a dry room, which is why migratory antistatic additives are useless there and permanently conductive grades are mandatory for handling equipment. Nylons also become brittle in very dry conditions, so PA components that perform well in a normal workshop can crack in a dry room after weeks of service.
Metal Contamination Is a Hard Limit
· Iron, copper, and nickel particles can create internal shorts — avoid metal-filled compounds near the cell
· Avoid bronze and metal-powder filled polymers anywhere upstream of cell sealing
· Pigments and colourants should be verified for metal content
· Wear parts must not shed abrasive debris onto electrode or separator surfaces
· Static-dissipative grades reduce particle attraction and discharge risk
· Use metal-detectable grades only where the detection system is downstream of the cell
Solvent and Electrolyte Resistance
NMP used in electrode coating softens many polymers, and the electrolyte — typically a lithium salt in a mixture of cyclic and linear carbonates — attacks others. PTFE, PFA, and PVDF handle the electrolyte well; PEEK and PPS handle NMP and the thermal load of drying. Polycarbonate and polystyrene are unsuitable near either. Moisture is the second half of the problem: electrolyte reacts with water to form hydrofluoric acid, so every polymer in the fill area should be selected for low moisture permeability as well as chemical resistance.
Sourcing for Line Builders
Battery lines are built fast and revised often, which favours machined polymer components over tooling investment. NAGOMER machines PEEK, PPS, POM, PTFE, and PFA components for coating, slitting, stacking, and filling equipment, and supplies stock shapes for fabricators building dry-room and electrolyte handling systems. Where conductivity is required, dissipative grades are available with resistivity certification.
Related reading: Antistatic and Conductive ESD Plastics, Plastics for EV Charging Infrastructure, and PEEK Grades Explained.
FAQ
Q1: What plastics are used in battery cell manufacturing?
PEEK and PPS for high-temperature and solvent-exposed positions, POM for wear parts, PTFE and PFA for electrolyte contact, and PPS or PBT for electrical insulators.
Q2: Why do antistatic additives fail in dry rooms?
Migratory antistatic additives depend on atmospheric moisture to form a conductive surface layer. At very low dew points they cannot function, so permanently conductive grades are required.
Q3: Can metal-filled plastics be used in battery plants?
Only well away from the cell. Metal particles create short-circuit risk, so bronze and metal-powder filled compounds are avoided upstream of sealing.
Q4: Which polymer resists electrolyte?
PTFE, PFA, and PVDF are the standard choices for electrolyte contact. PEEK and PPS handle NMP and drying temperatures.
Q5: Why is moisture control so critical?
Electrolyte reacts with water to form hydrofluoric acid, which degrades the cell and attacks materials. Low permeability polymers and dry-room assembly both address this.
Building battery production equipment? Contact NAGOMER for PEEK, PPS, PTFE and PFA components to drawing.
────────────────────────────────────────
NAGOMER — Professional Engineering Plastics Solutions
www.noegem.com | info@noegem.com