PPS (Polyphenylene Sulfide): Properties, Grades and Applications

Property Profile

Property

Unfilled PPS

GF40 PPS

PEEK (reference)

Continuous service (°C)

~200

~200–220

~250

Melting point (°C)

~280

~280

~343

Chemical resistance

Excellent

Excellent

Excellent

Tensile strength

Moderate

High

High

Impact strength

Low

Low

Good

Flame retardancy

Inherent V-0

Inherent V-0

Inherent V-0

Water absorption

Very low

Very low

Low

Relative cost

Medium

Medium

High

 

Chemical Resistance Is the Headline

PPS resists virtually all solvents, fuels, oils, and most acids and alkalis below about 200°C — a chemical range that only fluoropolymers exceed. Combined with very low water absorption, this makes it unusually predictable: a PPS part holds its dimensions and properties in hot oil, in brake fluid, in refrigerants, and in process chemistry, without the swelling or hydrolysis that limit polyamides and polyesters. In automotive fluid systems and chemical plant instrumentation, that predictability is often the deciding factor.

ngm s12n pps (12)

Unfilled versus Glass Filled

· Unfilled PPS is brittle — use it only where chemical purity or electrical properties dominate

· GF40 (40% glass) is the standard engineering grade: strong, stiff, dimensionally stable

· Mineral-filled and GF/mineral hybrids improve dimensional stability further for precision housings

· Carbon-filled grades add ESD performance and thermal conductivity

· All grades are inherently flame retardant without additives

· Glass-filled grades are abrasive to tooling and brittle at notches — design radii generously

 

PPS also behaves unusually in fire: it is inherently flame retardant and produces relatively little smoke, without the halogenated additives that complicate compliance in electronics and transport. That property alone explains a large share of its connector and housing volume, since it removes an entire additive package from the qualification. Combined with very low water absorption, it is one of the few materials that satisfies electrical, chemical, and fire requirements simultaneously.

Where PPS Is the Default Choice

· Automotive fluid systems — fuel, cooling, and brake components in contact with hot fluids

· Electrical connectors and housings needing V-0 plus dimensional stability

· Chemical plant instrumentation, valve internals, and pump components

· Oil and gas downhole electronics housings and sensor bodies

· Aerospace brackets and clips requiring flame retardancy plus chemical resistance

· Refrigeration and compressor components in contact with lubricants

 

Machining and Design Notes

PPS machines cleanly but is unforgiving of stress concentrations: unfilled grades in particular crack at sharp internal corners and over-torqued threads. Generous radii, piloted bosses instead of bare threads, and stress-relief annealing after rough machining address most of it. Its low water absorption is an advantage for tolerance control — a machined PPS part holds its dimensions in humid service where a nylon part would drift. NAGOMER supplies PPS sheet, rod, and tube in unfilled, glass-filled, and carbon-filled grades, machined to drawing with material certification.

Related reading: PEEK Grades Explained, Plastics for Automotive Under-Hood Applications, and High Voltage Insulation Plastics.

防静电 peek

FAQ

Q1: What temperature can PPS handle?

Around 200°C continuous, with inherent flame retardancy to V-0 without additives.

Q2: Is PPS better than PEEK?

It is cheaper and chemically excellent, but weaker, less tough, and limited to about 200°C. Above that, or where impact matters, PEEK is the better material.

Q3: Why is unfilled PPS rarely used?

It is brittle. Glass-filled grades provide the strength and stiffness that make PPS practical in most applications.

Q4: Does PPS absorb water?

Very little — among the lowest of engineering plastics, which keeps machined dimensions stable in humid service.

Q5: Can PPS replace nylon in fluid systems?

Often yes, and usually better: PPS resists hot fluids without the swelling and hydrolysis that affect polyamides.

Need PPS in unfilled, GF40 or carbon-filled grades? Contact NAGOMER for stock shapes and machined parts.

────────────────────────────────────────