Creep and Relaxation Explained

Creep is increasing deformation under constant load: hang a weight on a plastic bar and it stretches further every month. Stress relaxation is the mirror image — hold a plastic part at fixed deformation and the force it exerts falls over time. A plastic screw or snap-fit experiences relaxation; a plastic beam supporting a static load experiences creep. Both accelerate sharply with temperature: raising the service temperature by 10°C can roughly double the creep rate, which is why a design validated at 20°C may fail at 50°C.

Material Behaviour Under Sustained Load

Material

Creep Resistance

Notes

PEEK (unfilled / filled)

Excellent

Best of common engineering plastics

PAI

Excellent

High strength retained under load

PPS / PPSU

Very good

Good dimensional stability under load

POM-C

Good

Predictable, widely characterised

PA66

Moderate

Moisture softens and accelerates creep

PC

Moderate

Temperature sensitive above 80°C

PTFE (unfilled)

Poor

Severe cold flow — always use filled grades

k12n (25)

Design Techniques That Work

· Reduce sustained stress — design for 20–30% of short-term allowable stress where creep matters

· Add ribs or supports to shorten unsupported spans without adding mass

· Use filled grades — glass and carbon fibre cut creep dramatically

· Distribute load over larger areas rather than concentrating it at bosses

· For bolted joints, use a metal washer or a compliant element that maintains preload

· Where a joint must stay tight, design in a spring element instead of relying on plastic stiffness

Testing Rather Than Assuming

Short-term tensile data tells you almost nothing about long-term behaviour. Real creep data is expressed as isochronous stress-strain curves or 1000-hour creep modulus values, measured to ISO 899. Where published data is unavailable, a simple load test at service temperature — a weight hung on a prototype for a few weeks — often reveals more than any datasheet. For safety-critical parts, consider accelerated testing at elevated temperature and use the resulting trend, not a single data point, to judge whether the design will hold for its intended life. NAGOMER can supply material data and machined test specimens to support that programme.

Related reading: Thermal Expansion & Dimensional Stability, PEEK Filled Grades Guide, and Bearings & Bushings Material Selection.

k12 (23)

FAQ

Q1: What is the difference between creep and stress relaxation?

Creep is increasing strain under constant stress. Stress relaxation is decreasing stress under constant strain. Both stem from the same molecular movement, and both worsen with temperature.

Q2: Which plastic has the best creep resistance?

Filled PEEK offers the best combination of creep resistance and temperature capability, followed by PAI and PPS. Unfilled PTFE is the worst — it cold-flows under modest sustained load.

Q3: How does temperature affect creep?

Creep rate roughly doubles for every 10°C increase in service temperature. This is why creep must always be evaluated at the maximum operating temperature, not at ambient.

Q4: Do glass-filled grades reduce creep?

Yes, substantially. Fibre reinforcement carries load that the polymer matrix would otherwise relax, cutting long-term deformation several-fold.

Q5: How is creep data measured?

ISO 899 tensile creep testing produces isochronous stress-strain curves and creep modulus values at defined times and temperatures. Ask suppliers for data at your service temperature.

Designing for long-term load? Contact NAGOMER for creep data and machined test specimens in PEEK, PPS, and POM.

────────────────────────────────────────

NAGOMER — Professional Engineering Plastics Solutions

www.nagomer.com  |  info@nagomer.com

滚动至顶部

Inquiry form