What Outgassing Means in Practice

Outgassing is the release of absorbed gases, water, and volatile constituents from a material under vacuum. It is quantified by the ASTM E595 test, which reports two figures: Total Mass Loss (TML) and Collected Volatile Condensable Materials (CVCM). The space and semiconductor industries generally require TML below 1.0% and CVCM below 0.1% — the CVCM figure matters most, since it measures what condenses onto nearby cold surfaces such as optics.

Material Selection for Vacuum Service

Material

Outgassing Behaviour

Vacuum Suitability

Polyimide (PI)

Very low TML and CVCM

The vacuum benchmark — insulators, spacers

PEEK

Very low; bakeable

Structural parts, carriers, insulators

PEI (ULTEM)

Low

Transparent, dimensionally stable parts

PPS / PPSU

Low

Chemical-exposed vacuum positions

PTFE

Moderate; higher permeability

Seals only; avoid near optics

PA66

Poor — absorbs and releases water

Avoid; long pump-down

POM

Poor — releases formaldehyde

Avoid in high vacuum

 

k12b (5)

Design Rules for Vacuum Components

· Bake parts before service to drive off absorbed water — most pump-down delay is water desorption

· Avoid trapped volumes and blind threads that vent slowly through narrow paths

· Specify low-outgassing grades with test certificates rather than assuming by polymer family

· Keep elastomers to a minimum, and prefer metal or polymer seals designed for the duty

· Mind thermal cycling: repeated bake-outs can change dimensions and stress state

 

Applications and Testing

In semiconductor and research vacuum systems, the standard applications for engineering plastics are insulators, spacers, wafer carriers, and low-friction slides — positions where metal would add mass, generate particles, or disturb fields. PI and PEEK dominate because they combine low outgassing with radiation resistance and mechanical stability through bake-out cycles. For any critical application, insist on ASTM E595 test data for the specific grade rather than the polymer family, and condition the parts by vacuum baking before installation: an un-baked component can dominate the system pump-down curve for hours. NAGOMER supplies certified PEEK, PI, and PEI stock shapes and machines vacuum-grade components to drawing with full material traceability.

Particle generation deserves equal attention. In semiconductor vacuum tools, particles decide yield, and most particles from plastic components come from sliding contact or from machining debris that was never removed. Specify cleanroom-compatible cleaning after machining, avoid sliding polymer pairs against each other, and choose hard, filled grades where contact is unavoidable. Combined with low outgassing and bake-out discipline, this is what separates a component that works in vacuum from one that merely survives it.

Related reading: Polyimide (PI) Plastic Guide, PEEK Sheet Properties, and PEEK in Semiconductor Manufacturing Equipment.

pei

FAQ

Q1: What is the ASTM E595 outgassing test?

A 24-hour vacuum exposure at 125°C that reports Total Mass Loss (TML) and Collected Volatile Condensable Materials (CVCM). Most space and semiconductor specifications require TML <1% and CVCM <0.1%.

Q2: Why is POM unsuitable for vacuum?

POM releases formaldehyde under vacuum and heat, contaminating the system and slowing pump-down. Use PEEK, PI, or PEI instead.

Q3: Why does pump-down take so long with plastics?

Usually water desorption. Plastics absorb atmospheric moisture, and under vacuum it leaves slowly. Vacuum baking parts before service removes most of the delay.

Q4: Is PTFE safe to use in vacuum systems?

For seals and low-duty positions, yes, but its outgassing and permeability are higher than PEEK or PI, so avoid it near optics or in high-vacuum measurement zones.

Q5: Can plastic parts survive bake-out cycles?

PEEK, PI, PEI, and PPS tolerate typical vacuum bake-outs at 120–200°C. Check glass transition and thermal expansion for the specific grade and cycle.

Building vacuum or semiconductor equipment? Contact NAGOMER for certified low-outgassing PEEK, PI, and PEI components.

────────────────────────────────────────

NAGOMER — Professional Engineering Plastics Solutions

www.nagomer.com  |  info@nagomer.com