News Centre
News Type
Send your inquiry
Plastics for Oil & Gas: Downhole Seals, Back-up Rings and Components
The Downhole Environment
Four stressors act together. Temperature degrades the polymer and accelerates ageing. Pressure drives gas into the material, so rapid depressurisation causes explosive decompression — internal gas expands faster than the polymer can diffuse it, blistering or splitting the seal. Produced fluids swell elastomers and attack certain polymers. And sour service, hydrogen sulphide plus CO2 plus water, is aggressively corrosive to many materials, with added risk of rapid gas decompression damage. A material that handles any three of these can still fail on the fourth, which is why qualification testing must reproduce the actual well conditions rather than a generic standard.
Material Map
Material | Max temp. | Strength | Notes |
PTFE (filled) | < 260°C | Low | Chemical inert, cold flows, needs back-up rings |
PEEK | 250°C+ | High | Standard for back-up rings and high-pressure seals |
PPS | ~200°C | Moderate | Good chemical resistance, lower cost than PEEK |
PAI (Torlon) | ~260°C | Very high | Excellent for bushings and bearing components |
PCTFE | < 200°C | Moderate | Very low permeability, used for barriers |
FEP / PFA | < 200°C | Low | Chemical resistance, low-temperature sealing |
PA11 / PA12 | ~90°C | Moderate | Flexible lines, lower-temperature duty |
Explosive Decompression and Gas Permeability
Under high pressure, gas dissolves into the polymer. When pressure is released quickly, the dissolved gas expands and the material can blister, crack, or delaminate. Dense, high-modulus polymers resist this far better than soft or highly filled ones: PEEK back-up rings and filled PTFE seals with low void content are preferred in gas service, and qualification to NORSOK M-710 or ISO 23936-2 includes a rapid gas decompression cycle precisely because it is a common failure mode. Seal geometry matters too — thicker sections retain gas longer and fail more readily than thin ones.
Seal Systems and Back-up Rings
· PEEK back-up rings prevent extrusion of elastomer seals at high pressure and temperature
· Filled PTFE (glass, carbon, graphite) provides low friction in dynamic sealing
· Anti-extrusion devices should be matched in modulus to the seal they protect
· Consider thermal expansion of the polymer against the metal housing over the full temperature range
· In sour service, verify the specific grade against the well chemistry, not the generic datasheet
· Design for replaceability — downhole components are maintained, not discarded
Qualification and Standards
The standards that matter are application-specific: NORSOK M-710 for elastomer and polymer seals in oil and gas, ISO 23936 series for polymers in contact with well fluids, API 6A and 17D for wellhead and subsea equipment, and client-specific ageing programmes that immerse samples in actual or synthetic produced fluids at temperature. A supplier who can document ageing data, decompression testing, and lot traceability is worth more than one who quotes a headline temperature rating. NAGOMER machines PEEK, PPS, PAI, and filled PTFE components for downhole and surface oilfield equipment to drawing.
Related reading: Plastics for Hydrogen Energy, Plastics for Chemical Processing Plants, and PAI (Torlon) vs PEEK.
FAQ
Q1: What is explosive decompression in polymer seals?
Gas absorbed under pressure expands rapidly when pressure drops, blistering or cracking the seal. Dense, high-modulus materials and thin sections resist it better.
Q2: Which plastic is best for downhole back-up rings?
PEEK is the standard choice for high pressure and temperature because of its modulus, creep resistance, and dimensional stability.
Q3: What temperature can PTFE seals handle downhole?
Around 260°C, but PTFE cold flows under load, so it is normally used with PEEK or metal back-up rings.
Q4: What is NORSOK M-710?
A Norwegian oil and gas standard for qualification of polymer and elastomer seals, including rapid gas decompression and ageing in well fluids.
Q5: Can standard grades be used in sour service?
Only after verification. Sour service requires grade-specific ageing data in H2S-containing fluids at temperature; generic datasheets are not sufficient.
Sourcing downhole polymer components? NAGOMER machines PEEK, PPS, PAI, and filled PTFE to specification.
────────────────────────────────────────
NAGOMER — Professional Engineering Plastics Solutions
www.nagomer.com | info@nagomer.com